Product Highlights : Low viscosity bonder. Used in gems and metal bonding for bracelets, necklaces, rings, penchants, hair clips, hair bands, earrings, crowns etc. Also used as dome coating of nameplates and logos.

Substrates              : -

Color                       : Water-White Clear

Viscosity                 : 700 - 1,400 cps

Tensile (psi)           :4,700 - 5,200

Hardness               : D83 to D93

Elongation             :  30%

 