TC-9042-1PINT
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Thermally Conductive, Aluminum-Filled, and Two Part Epoxy Paste
Ratio : 100:12
Color : Grey
Viscosity Mixed (cP) : 10,000
Volume Resistivity (ohms-cm) : 1.0 x 105
Dielectric Strength (volts/mil) : 50
Thermal Conductivity (Btu-in/hr-ft2-°F) : 12.5
Temp. Resistance (°C) : 300