TC-9042-1PINT

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights                                     : Thermally Conductive, Aluminum-Filled, and Two Part Epoxy Paste

Ratio                                                             : 100:12

Color                                                            : Grey

Viscosity Mixed  (cP)                                  : 10,000

Volume Resistivity (ohms-cm)                  : 1.0 x 105

Dielectric Strength (volts/mil)                   : 50

Thermal Conductivity (Btu-in/hr-ft2-°F)   : 12.5

Temp. Resistance (°C)                                : 300

 