CM-2500-50GM
Product Availability: 2 To 4 Weeks
Product Highlights : High Temp., High viscosity, Rubber toughened, Bonds P,R,M,F,C,W and Medical/Military grade
Substrates : Ultra-High Temp, Superior Strength Cyanoacrylate Bonder
Viscosity : 2,500 cps
Color : Clear
Bonding Strength (psi)
ABS : 2,500
Aluminum : 3,200
PC : 3,800
PVC : 3,200
Rubber : 2,200
Steel : 5,200