Product Highlights :

Medium high viscosity, superior high strength bonder. Used for bonding of metals, glass and ceramics in electronics/optical/medical devices. Very low shrinkage and water absorption. Ability to withstand stringent thermal cycling.

Substrates              : High Performance Metal/Glass/Ceramics

Color                       : Clear Transparent

Viscosity                 : 4,500 - 7,500cps

Tensile (psi)            : 10,100-12,600

Hardness                : D80 - D90

Elongation              :  24%

 