UHTE-5320-5GAL

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights              : Two Part Epoxy, 1:1 Ratio System for Tough Bonding Applications.

Color                                     : Amber

Dielectric Strength              : 450 volts/mil

Viscosity (cPs)                     : 6,000 – 10,000

Hardness Shore                   : D89

Vol. Resistivity (ohms-cm) : 4.0 x 1014

Chemical Resistance           : Good

 