HTE-6468-50GM
Product Highlights : Two-component epoxy (sealant and encapsulant) bonding material. 3 mins fast-setting, strength
starts increasing after 15 mins, full cure in 72hrs. High gloss black encapsulant, high temperature
and chemical resistance.
Substrates : Multi-Substrates (High Strength)
Color : Black Glossy
Tensile (psi) : 9,400
Flexural (psi) : 145,400
Viscosity (Mixed) : 12,500 cps
Cure (Shrinkage) : 0.0005 in/in
Temperature (Resistance) : -55 to 155°C