HTE-5350-1GALLON

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights                 : Two-part epoxy system designed for bonding and potting applications operating at high temperatures.
                                                   Bonds various substrates, with exceptional chemical resistance. Outstanding performance within
                                                   operating temperature range.

Substrates                              : Multi-Substrates

Color                                       : Grey

Tensile (psi)                           : 2,500

Flexural (psi)                         : 11,400 

Viscosity  (Mixed)                  : Paste

Cure (Shrinkage)                   : 0.002 in/in

Temperature  (Resistance)   : -65 to 204°C

 