Product Highlights : Cost efficient epoxy-acrylate, thick viscosity, ultra-low shrinkage and water absorption potting compound for use
                                   in sensitive electronic devices. UV / Heat curable. Chemical and vapor resistance.

Substrates              : Multi-Substrates (Metal/Glass/Ceramics)

Color                       : Clear

Viscosity                 : 6,000 cps

Tensile (psi)           : 1,700 - 5,600

Hardness                :  D55 – D65

Elongation             :  160%

 