1238
Product Availability: 2 To 4 Weeks
Product Highlights : Very high strength, high viscosity metal / glass bonder. Very low water absorption and linear shrinkage.
Fast-curing and ideal for bonding all types of glass panels to stainless steel structures in general industries.
Substrates : High Performance Metal/Glass/Ceramics
Color : Clear
Viscosity : 21,000 cps
Tensile (psi) : 5,700 - 8,900
Hardness : D75 – D85
Elongation : 76%