Product Highlights : Multi-substrate bonding gel for most plastics, metal and glass. Ideal for out-door bonding in general and
                                    construction industries. Good passive vibration resistance. Enhanced thermal and water resistance.

Substrates              : Multi-Substrates (High Strength Plastics)

Color                       : Clear

Viscosity                : 53,000 cps

Tensile (psi)           : 3,700 - 6,900

Hardness               : D63 – D73

Elongation             :  260%

 