1435-5GALLON

Product Availability: 2 To 4 Weeks

Product Highlights :  A very fast curing, high strength plastic bonder for PVC / PC / ABS / Polyester / Ultem and many different
                                     plastics. Highly flexible, it is used also in the sealing of test-tubes. High temperature and thermal resistance.

Substrates              : Multi-Substrates (Plastics)

Color                       : Slight Yellow Tint

Viscosity                 : 4,500 cps

Tensile (psi)            :7,300

Hardness                : D55 - D65

Elongation              :  240%

 