CM-4-20GM

Product Availability: In stock

Product Highlights            : Low odor / Low bloom, Ultra-low viscosity, Solvent-resistant, Bonding P,R,M and Medical grade

Substrates                          : Ultra-low Odor,Non-Bloom, High Strength Medical CA Bonder

Viscosity                             : 4 cps

Color                                   : Clear

Bonding Strength (psi)

ABS                                    : 800

Aluminum                          : 2,300

PC                                      : 1,300

PVC                                    : 1,100

Rubber                              : -

Steel                                  : 3,000

 