Product Highlights            : Fasting setting, Medium-high viscosity, Solvent-resistant, Bonds P,R,M,F,C,W and Medical/Military grade

Substrates                          : High Strength, Fast Setting Medical CA Bonder

Viscosity                             : 1,800 cps

Color                                   : Clear

Bonding Strength (psi)

ABS                                    : 2,700

Aluminum                          : 520

PC                                      : 3,700

PVC                                    : 3,900

Rubber                              : 2,200

Steel                                  : 2,800

 