HTE-5354

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights                  : Two-part epoxy system for bonding and potting applications requiring good flexibility operating at
                                                    high temperatures. Bonds various substrates, delivers outstanding performance on application
                                                    within the operating temperature range. 

Substrates                               : Multi-Substrates

Color                                        : Clear

Tensile (psi)                            : 1,200

Flexural (psi)                          : 8,000

Viscosity  (Mixed)                  : 12,000 cps

Cure (Shrinkage)                   : 0.008 in/in 

Temperature  (Resistance)   : -50 to 200°C

 