HTE-5351

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights               : Two-part epoxy system for bonding and potting applications  operating at high temperatures. Bonds
                                                  various substrates. Meets NASA outgassing requirements.

Substrates                            : Multi-Substrates 

Color                                      : Amber

Tensile (psi)                          : 3,000

Flexural (psi)                         : 10,200

Viscosity  (Mixed)                  : 25,000 cps

Cure (Shrinkage)                   : 0.002 in/in

Temperature  (Resistance)   : -65 to 204°C

 

There are yet no reviews for this product.