Product Highlights                : Two-part epoxy system for repair and maintenance of applications operating at high temperatures.
                                                    Bonds various substrates.

Substrates                             : Multi-Substrates

Color                                      : Grey

Tensile (psi)                           : 2,500

Flexural (psi)                         : 12,000

Viscosity  (Mixed)                 : Paste

Cure (Shrinkage)                   : 0.002 in/in

Temperature  (Resistance)   : -65 to 204°C

 