864-3OZ
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Chemical Type : Oxime
Color : Clear
Viscosity : 400 – 600
Density (g/ml) : 0.99
Peel Strength (psi) : 300
Tensile Shear (psi) : 225
Elongation (%) : 325