905-3OZ
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured
adhesive in shadowed areas. Used as conformal coating and sealant for PCBA and electronic components.
Cure Time : 24 hr, RT
Viscosity : 600
Temp. Resistance (°C) : -45 to 260
Color : Clear
Tensile ( psi) : 100
Video