27
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : High Temp., High Strength, Heavy duty work, Vibration absorption and No surface preparation
Substrates : High-Temp Anaerobic Vibration Resistant Thread-Locker
Color : Clear Blue
Viscosity : 2,200 - 3,000 cps
Strength : Medium
Gap Fill : 0.007''
Break Torque (in-lbs) : 120 -170