Product Highlights :Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage
                                   and good passive vibration isolation capability. Resistant to moisture and low water absorption.

Color                       :Slight Tint

Viscosity                 : 20,500 cps

Tensile (psi)            :8,000 – 8,200

Hardness                : D43 - D53

Elongation              : 444%

 