HTCP-650-1QT

Product Availability: 2 To 4 Weeks
Price Shown Is Per Each (Ex-Work USA)

Product Highlights              : Thixotropic paste putty. Used to seal boiler doors and    molten metal systems. Easy to apply and
                                                removable.  For uses to 2300°F.

Color                                     : Brownish Grey

Viscosity                               : Paste

Number Component            : 1

Specific Gravity  (gms/cc)  : 1.27

Air Set (hrs)                         : 1 – 2

Heat Cure (°F, hrs)              : 200, 2-4

Max. Temp.  (°F)                  : 2,300

 

There are yet no reviews for this product.