IMG_1757615

1462-10GM

Product Availability: 2 To 4 Weeks

Product Highlights : Low viscosity, acid-free, multi-substrate / plastic bonder. For electronics industry. Good bonding strength on
                                   multiple substrates such as metals, glass and FR4 materials on a single application.

Substrates              : Low Adhesion Multi-Substrates (High Strength Plastics)

Color                       :Slightly Amber

Viscosity                 :450 cps

Tensile (psi)           :2,800 - 6,900

Hardness               :D49 – D59

Elongation            : 827%

 