3522-1KG
Product Availability: 2 To 4 Weeks
Product Highlights : Low viscosity encapsulant. Clear, hard, sleek and resilient protective coating thickness of 300 to 4,500 microns
on components. Very low water absorption.
Substrates : Low Adhesion
Color : Clear
Viscosity : 20 cps
Tensile (psi) : 150
Hardness : D84 – D94
Elongation : 4%