1933-10GM
Product Availability: 2 To 4 Weeks
Product Highlights : Very low Viscosity, UV / Visible light / LED / Heat-curing, high strength metal-glass bonder. Track free,used in
very high strength bonding application requiring good temperature and moisture resistance.
Substrates : High Strength Metal/Glass/Ceramics
Color : Slight Translucent
Viscosity : 700 cps
Tensile (psi) : 8,300 – 14,000
Hardness : D80 – D90
Elongation : 33%