9254-2GALLON

Product Availability: 2 To 4 Weeks

Product Highlights : Cures with UV / Visible / Heat or Actif 398. Very high strength, medium viscosity metal / glass bonder.
                                    Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption

Substrates              : High Performance Metal/Glass/Ceramics

Color                       : Slight Tint

Viscosity                : 1,850 cps

Tensile (psi)           : 16,000 - 9,500

Hardness               : D66 – D76

Elongation             :  60%

 