4201-300GM
Product Availability: 2 To 4 Weeks
Product Highlights : Aerospace Grade. Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal /
glass / ceramics masking material. Low linear shrinkage, good temperature and moisture resistance.
Substrates : High Performance Metal/Glass/Ceramics
Color : Slight Tint
Viscosity : 130 cps
Tensile (psi) : 7,400 – 10,000
Hardness : D75 – D85
Elongation : 4%