Product Highlights :Low viscosity and low water absorption electronics sealant. Provides air-tight seal with ease of peel for rework.
                                  Tough yet elongating. Widely use for automotive and electronics industries for its low CTE properties.

Substrates              : Very Low Strength Multi-Substrates

Color                       : Slight Translucent

Viscosity                 : 600 cps

Tensile (psi)            : 1,200 - 3,000

Hardness                : A5 – A15

Elongation              :  374%

 