Product Highlights : Flexible encapsulant for electronic devices. Cures in seconds with secondary hear cure option for hidden areas.
Bonds to many different substrates.
Substrates : MultiSubstrates
Color : Slightly Translucent
Viscosity :14,000 cps
Tensile (psi) : 2,400 - 5,200
Hardness : D40 – D50
Elongation : 254%