5422CF-30GM
Product Availability: 2 To 4 Weeks
Price Shown Is Per Each (Ex-Work Singapore)
Product Highlights :Color-change during cure from blue to clear. Low viscosity, multi-substrate bonder for most plastics, metal and
glass. Ideal for needle / reservoir / catheter / transducer assemblies in the medical industry. Meet ISO 10993-5.
Passes EtO & gamma sterilization.
Substrates : Multi-Substrates
Color : Clear, Fluorescing
Viscosity : 200 – 400 cps
Tensile (psi) :3,700 – 6,900
Hardness : D57 to D67
Elongation : 350%