3148-10GM
Product Availability: 2 To 4 Weeks
Product Highlights : Ultra-clean and tough. Very effective protection against chemical stains and scratch marks. No residue or
contamination after removal. Ideal for protection of critical surfaces during manufacturing processes.
Substrates : Good Strength Metal/Glass/Ceramics
Color : Dark Blue
Viscosity : 6,000 cps
Tensile (psi) : 4,600 – 5,300
Hardness : D49 – D59
Elongation : 250%