5300F-1KG
Product Availability: 2 To 4 Weeks
Price Shown Is Per Each (Ex-Work Singapore)
Product Highlights : Low viscosity, multi-substrate bonder for most plastics, metal and glass. Ideal for needle / reservoir / catheter /
transducer assemblies in the medical industry. Formulated to meet ISO 10993-5. Passes EtO & gamma
sterilization.
Color : Translucent
Viscosity : 105 cps
Tensile : 2,700 – 5,300 psi
Hardness : D73 - D83
Elongation : '8%