5422F-10GM

Product Availability: 2 To 4 Weeks
Price Shown Is Per Each (Ex-Work Singapore)

Product Highlights   : Low viscosity, multi-substrate bonder for most plastics, metal and glass. Ideal for needle / reservoir / catheter /
                                     transducer assemblies in the medical industry. Meet ISO 10993-5. Passes EtO & gamma  sterilization. 

Color                          : Clear, Fluorescing

Viscosity                   : 300 cps

Tensile                      : 3,700 - 6,900 psi

Hardness                  : D57 - D67

Elongation                : 350% 

 