1465-1GALLON
Product Availability: 2 To 4 Weeks
Product Highlights :Cures tack-free, it is a superior plastics / metals / glass / ceramics multi-substrate bonder. Ideal for applications
requiring minimal drift in positioning optics and devices with very low shrinkage property.
Substrates : High Strength Multi-Substrates
Color : Slight Translucent
Viscosity : 6,000 cps
Tensile (psi) : 5,400
Hardness : D60 - D70
Elongation : 105%