1827-2GALLON
Product Availability: In stock
Product Highlights : Industrial grade, multi-substrate, high viscosity bonder for metals / glass / plastics (elastomers). Very high
bonding strength. Low shrinkage and water absorption. Superior passive vibration absorption capability.
Substrates : Multi-Substrates (High Strength Plastics)
Color : Slight Yellowish Tint
Viscosity : 9500 cps
Tensile (psi) : 6,900
Hardness : D48 - D58
Elongation : 913%