1435-300GM
Product Availability: 2 To 4 Weeks
Product Highlights : A very fast curing, high strength plastic bonder for PVC / PC / ABS / Polyester / Ultem and many different
plastics. Highly flexible, it is used also in the sealing of test-tubes. High temperature and thermal resistance.
Substrates : Multi-Substrates (Plastics)
Color : Slight Yellow Tint
Viscosity : 4,500 cps
Tensile (psi) :7,300
Hardness : D55 - D65
Elongation : 240%