GENERAL PURPOSE

GENERAL PURPOSE CYANOACRYLATE ADHESIVES

Incure Quik-FixTM line of General Purpose Cyanoacrylate Adhesives offer the most diverse line of instant adhesives/cyanoacrylate glue available, providing you with fast assembly solutions for a variety of materials, including rubbers, plastics and metals. Cyanoacrylate is a one component, no mix product that cure rapidly at room temperature without heat or light, making it exceptionally easy to use.

Advantages of Quik-FixTM - Cyanoacrylate

  Single Component - Easy To Use
  Prevent Loosening from Shock and Vibration
  Reduce Inventory Costs - Used On Various Sizes
  Available in a Variety of Viscosities

Learn about our Light Curing Systems

C9000 / U8000 UV Light Curing Conveyor Systems
F100P / F200P Programmable UV Flood Curing Lamps
L1000 High Intensity UV LED Flood Lamps
L9000 Compact UV LED Spot Curing Lamps
S10 / S20 Ultra High Intensity Light-Curing Spot Lamps
Cyanoacrylate
Quik-FixTM Series Core Products
Product Product Highlights Substrates Viscosity Shear Strength Bonding Strength (psi)
ABS Aluminum PC PVC Rubber Steel  
101 • Ultra-fast setting
• Ultra-low viscosity
• Solvent-resistant
• Bonds P,R,M
High Strength,
Fast Setting
Structural CA Bonder
2 cP 3,400 psi 2,400 2,300 3,400 3,400 2,200  3,000
104 • Ultra-fast setting
• Low viscosity
• Solvent-resistant
• Bonds P,R,M
High Strength,
Multi-Substrates
Structural CA Bonder
110 cP 3,400 psi 2,400 2,300 3,400  3,400 2,200 3,000
105 • For porous materials
• Gel viscosity
• Ease of control
• Solvent-resistant
• Bonds P,R,M
High Strength,
Multi-Substrates
Structural CA Bonder
11,500 cP 3,875 psi 2,700 2,000  3,700 3,900 2,200 2,800
115 • Fast setting
• High viscosity
• Solvent-resistant
• Bonds P,R,M,F,C,W
High Strength,
Multi-Substrates
Structural CA Bonder
1,800 cP 3,400 psi  2,400 2,300 3,400  3,400 2,200  3,000
117 • Ultra-fast setting
• Medium viscosity
• Solvent-resistant
• Bonds P,R,M,F,C,W
• Medical/military grade
High Strength,
Multi-Substrates Structural CA Bonder
400 cP 3,875 psi  2,700  2,700 3,700 3,900 2,200 2,800
Package Size: 20g bottle / 500g bottle
Abbrv: P - Plastics, R - Rubber, M - Metals, F - Foam, C - Cloth, W - Wood

Results 7 - 10 of 10
115-20GM

Product Highlights            : Fast ...

$12.79