880-11OZ

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Chemical Type           : Oxime

Color                           : Translucent

Viscosity                     : 800 – 1,200

Density  (g/ml)            : 1.02

Peel Strength (psi)     : N.A.

Tensile Shear  (psi)    : 220

Elongation (%)           : 315

 