CM-15-50GM
Product Availability: 2 To 4 Weeks
Product Highlights : Ultra-fast setting, low viscosity, Solvent-resistant, Bonding P,R,M and Medical/Military grade
Substrates : High Strength, Fast Setting Medical CA Bonder
Viscosity : 15 cps
Color : Clear
Bonding Strength (psi)
ABS : 2,700
Aluminum : 520
PC : 3,700
PVC : 3,900
Rubber : 2,200
Steel : 2,800