Product Highlights            : Ultra-fast setting, low viscosity, Surface insensitive, Bonding P,R,M and Medical/Military grade

Substrates                          : High Strength, Fast Setting  Medical CA Bonder

Viscosity                             : 105 cps

Color                                   : Clear

Bonding Strength (psi)

ABS                                    : 2,600

Aluminum                          : 2,400

PC                                      : 4,100

PVC                                    : 3,600

Rubber                              : 2,200

Steel                                  :  2,500

 