1453-1GALLON
Product Availability: 2 To 4 Weeks
Product Highlights : Uniquely high elongation provides extra-ordinary bonding of different hardness layers for the construction of
sport-courts, cushion carpets etc. High strength plastics bonder with good vibration isolation capability.
Substrates : Multi-Substrates (High Strength Plastics)
Color : Slight Yellow Tint
Viscosity : 700 cps
Tensile (psi) : 6,900
Hardness : D45 - D55
Elongation : 860%