UV MASK

LIGHT CURABLE PEELABLE MASKS FOR SURFACE PROTECTION AND PARTS HANDLING ASSEMBLY

Incure LitemaskTM offers a unique range of temporary UV peelable masks for MRO, electronics and orthopaedic industry. These UV/visible light curable materials’ resilience, strong adhesion and chemical resistance prevents edge lift and yet preserves the integrity of the surface being protected. Simplify your process by eliminating long masking cycles.

Fill in your Masking Application Profile Here


Peelable Mask
Temporary Masking Resins
Orthopadic Mask
Advantages of LitemaskTM - Peelable Masks

   Apply, Cure and Remove in Seconds!

   Residue Free Removal  
   Applied by Coating, Dipping or Spraying
Learn about our Light Curing Systems

C9000/ U8000 UV Light Curing Conveyor Systems
L9000 Compact UV LED Spot Curing Lamp
S10 / S20 Ultra High Intensity Light-Curing Spot Lamps
LitemaskTM Series Core Products
Product Product Highlights Substrates Color Viscosity  Tensile (psi) Hardness Elongation  
4201 Aerospace Grade. Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics masking material. Low linear shrinkage, good temperature and moisture resistance. High Performance 
Metal / Glass / Ceramics
Slight Tint 130 cP 7,400 
to
10,000
D75 – D85 4%
4272 Aerospace Grade. Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics masking material. Low linear shrinkage, good temperature and moisture resistance. High Performance 
Metal / Glass / Ceramics
Slight Tint 400 cP 9,700 
to
10,900
D77 – D87 4%
4153 Ultra-clear, low viscosity UV / Visible Light / LED / Activator / Heat-curing, high strength metal-glass mask for protection of surfaces during blasting. Remove by burn-off. Tack-free, used in jewelry industry. High Performance 
Metal / Glass / Ceramics
Slightly Translucent 700 cP 7,000 
to
8,400
D80 – D90 33%
3148 Ultra-clean and tough. Very effective protection against chemical stains and scratch marks. No residue or contamination after removal. Ideal for protection of critical surfaces during manufacturing processes.  Good Strength 
Metal / Glass / Ceramics
 Dark Blue 6,000 cP 4,600 
to
5,300
D49 – D59 250%
4139 Cures with UV / Visible / Heat or Actif 398. Very good adhesion to metals and glass. Used in aerospace industry for the effective protection of turbine blades against chemicals during cleaning. High Performance 
Metal / Glass / Ceramics 
 Clear 24,000 cP 9,800 
to
16,000
D75 – D85 55%
8114VT Very high viscosity, ultra-clean peel-able high temp mask for electronics and aerospace industries.  Soft, tough and flexible for surface protection against chemical stains and burnt marks during manufacturing processes. Peelable  Clear 
Transparent
25,000 cP 100
to
1,600
D30– D40 26%
Above products are available in thicker versions: T (Thick), VT (Very Thick), G (Gel)
Package Size: 10 ml syringe / 30 ml syringe / 30 ml squeeze bottle / 100 ml squeeze bottle / 250 ml squeeze bottle / 1 kg Bottle / 1 Gallon Pail / 2 Gallon Pail / 5 Gallon Pail

 

APPLICATION:
Peelable Mask
1. Apply at locations that needs to be protected

PCB Masks
Removal of Litemask from PCB board.
UV light Source
2. Cure Litemask with F500 UV lamp

PBC Coatings
Click image to watch removal of LitemaskTM
UV Mask
3. Peel off easily. No residue.

UV Peelable Mask
Click image to watch demostration.

 

Results 37 - 42 of 42
4201-2GALLON

Product Highlights : Aerospace Grade. ...

$847.50
4201-1GALLON

Product Highlights : Aerospace Grade. ...

$474.88
4201-1KG

Product Highlights : Aerospace Grade. ...

$161.38
4201-300GM

Product Highlights : Aerospace Grade. ...

$103.69
4201-30GM

Product Highlights : Aerospace Grade. ...

$31.69
4201-10GM

Product Highlights : Aerospace Grade. ...

$17.19