Product Highlights :  A straw color gel silicone that is removable after cure. Clean release from plastics, metals and painted wood. Non-corrosive.

Color                       : Translucent

Appearance            : Gel

Viscosity                 : 80,000

Tensile (psi)            :100

Hardness                : A30

 