Product Highlights         : A straw color liquid silicone that is removable after cure. Clean release from plastics, metals and painted
                                           wood. Non-corrosive.

Color                                : Translucent

 Appearance                   : Liquid

Viscosity (cP)                 : 40,000

Hardness (Shore)          : A20

Tensile Strength ( psi)  : 100

 