TC-9033
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Thermally Conductive, Aluminum-Filled, and 1:1 Epoxy Paste
Ratio : 1:1
Color : Grey
Viscosity Mixed (cP) : Paste
Volume Resistivity (ohms-cm) : 1.0 x 105
Dielectric Strength (volts/mil) : 80
Thermal Conductivity (Btu-in/hr-ft2-°F) : 9.0
Temp. Resistance (°C) : 204