Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Filler                                                 : Alumina

Color                                                 : White

Chemical Resistance                     : Excellent

Thermal Conductivity (W/m-°K)    : 0.475

Specific Gravity (gms/cc)              : 2.42

Dielectric Strength  (volts/mil)     : 300

Volume Resistivity (Ohms-cm )    : 1014

Temperature Limit  (°F)                 : -60 to 550

 