TCG-40
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Filler : Copper
Color : Copper
Chemical Resistance : Excellent
Thermal Conductivity (W/m-°K) : 4.68
Specific Gravity (gms/cc) : 1.33
Dielectric Strength (volts/mil) : 4
Volume Resistivity (Ohms-cm ) : 103
Temperature Limit (°F) : -60 to 550