Thermally & Electrically Conductive Adhesive — Epo-Weld™
Nickel-filled and silver-filled 2-part epoxy adhesives for EMI/RFI shielding, grounding, and high-performance electronic bonding. TEC-9015 delivers cost-effective nickel conductivity for shielding gaskets and grounding straps; TEC-9017 delivers premium silver conductivity for low-resistance LED and electronic component bonds.
Technical Specifications
Built for Conductive Electronic Bonding
Epo-Weld™ TEC-9015 and TEC-9017 address two distinct conductive bonding requirements —
cost-effective nickel EMI shielding and premium silver conductivity for high-performance assemblies.
Frequently Asked Questions
Common questions about Epo-Weld™ TEC conductive epoxy adhesives.
-
Epo-Weld™ TEC is a 2-part epoxy providing simultaneous thermal and electrical conductivity. It is used in EMI/RFI shielding enclosures, grounding straps, heat sink bonding, LED attachment, and electronic component assembly.
-
TEC-9015 is nickel-filled (dark gray) and designed for cost-effective EMI/RFI shielding, grounding, and heat sink bonding — with higher viscosity (90,000–120,000 cps) suited to vertical surfaces. TEC-9017 is silver-filled (light brown) and delivers premium, low-contact-resistance conductivity for LED and electronic component bonding, with moderate viscosity (48,000–65,000 cps).
-
Epo-Weld™ TEC offers three cure schedule options: 24 hours at room temperature (77°F), 2 hours at 100°F, or 1 hour at 200°F. Select the schedule that fits your production process or equipment constraints.
-
Yes — Epo-Weld™ TEC-9015 (nickel-filled) is engineered specifically for EMI/RFI shielding. Its nickel filler provides stable electrical conductivity and magnetic shielding properties, replacing solder or mechanical clips with a durable, corrosion-resistant conductive bond.
-
Yes — Epo-Weld™ TEC is commonly used as a solder replacement in heat-sensitive assemblies or flexible substrates. TEC-9017's silver filler provides low contact resistance comparable to solder, while curing at temperatures far below solder reflow.
-
Epo-Weld™ TEC is rated for continuous service up to 200°F (93°C). Both TEC-9015 and TEC-9017 maintain their conductive and structural properties through repeated thermal cycling within this range.