Back to S20™ S20™ 1-Pole — Technical Datasheet

S20™ 1-Pole — Single-Point UV Arc Spot Curing Lamp

Incure S20-1P channels the S20™'s full >21 W/cm² UVA output to a single lightguide tip — no splitting, no intensity loss. Powered by a 200W mercury arc lamp with broad-spectrum 300–550 nm output and a programmable 1–99 second timer, the S20-1P delivers the highest per-tip irradiance in the S20™ range. Available with Ø3, Ø5, and Ø8 mm lightguide tips in lengths from 0.5 m to 6.2 m for single-point bonding, fibre optic connectors, needle hub assembly, and precision component curing.

>21 W/cm² UVA at Source

All S20™ lamp output directed to one lightguide tip — no power division, no intensity loss. Delivers exceptionally high UVA irradiance for rapid curing, reduced cycle times, and effective curing of thicker adhesive bond lines and highly filled formulations.

Compatible with Any UV-Curable Adhesive

Broad-spectrum 300–550 nm output covers UV and visible wavelengths, activating all standard photoinitiator systems — no adhesive reformulation or compatibility testing required.

Widest Tip Selection in the S20™ Range

Available with Ø3, Ø5, and Ø8 mm lightguide tips in lengths from 0.5 m to 6.2 m — including the Ø8 mm maximum-aperture tip only possible on a single-output configuration. UV protective safety goggles included.

Incure S20™ 1-Pole single-output UV liquid lightguide
Specifications
ModelS20-1P
100–120 VAC200–240 VAC
AC Input Voltage100–120VAC ±10%200–240VAC ±10%
AC Input Current4.7 Amperes2.5 Amperes
Source Input Frequency47 Hz to 63 Hz
Lamp Power Regulation±1.0%
Fan / Auxiliary Voltage24V @ 0.5A
Lamp Type200 Watt Mercury Arc
Burning PositionHorizontal
Radiation Flux300–550 nm
Warm-up Time1 to 2 minutes
Cooling Time Before Restart2 to 5 minutes typical
Output Intensity (Typical)>21 W/cm² UVA (at source)
Output Intensity Range25–100% adjustable
Timer Range1–99 seconds (programmable)
Lamp Life>2,000 hours typical
Operating Temperature+10°C to +40°C / +50°F to +104°F
Relative Humidity30–75% operating, 10–100% storage
CoolingDual DC Fans, Filtered
Over-temp Shutdown65°C (internal)
Lightguide Configuration — S20-1P
Lightguide PolesSingle-Pole (1 Output)
Lightguide TypeUV Liquid Lightguide
Tip Diameters AvailableØ3 mm, Ø5 mm, Ø8 mm
Lightguide Lengths0.5 m, 1 m, 1.5 m, 2 m, 3 m, 6.2 m (custom available)
Physical
L × W × H (Controller)10.6" × 8.7" × 4.1"
Weight6.0 lbs (2.7 kg)
Safety EquipmentUV Protective Goggles Included
Ordering
P/N FormatS20-1P-[Diameter]-[Length]
Diameter Code3 / 5 / 8
Length Code (mm)500 / 1000 / 1500 / 2000 / 3000 / 6200
Example P/NS20-1P-3-500

Output intensity is measured at the lightguide tip with the system operating at 100% power. Actual irradiance may vary depending on lightguide length, tip diameter, and the condition of the lightguide and optical components.